Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
Average value: 6.00 µm/m-°C Grade Count:6
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
CTE, linear, Transverse to Flow 6.00 - 55.0 µm/m-°C
3.33 - 30.6 µin/in-°F
Average value: 47.4 µm/m-°C Grade Count:38
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
CTE, linear, Transverse to Flow 6.00 µm/m-°C

@Temperature 25.0 - 1500 °C
3.33 µin/in-°F

@Temperature 77.0 - 2730 °F
Perpendicular to pressing direction
Momentive Performance Materials HBN Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..
CTE, linear, Transverse to Flow 6.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66
LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 6.00 µm/m-°C

@Temperature 23.0 - 150 °C
3.33 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
DuPont Performance Polymers VESPEL TP-8474 Polyimide
DuPont Vespel TP-8474 parts are specified for mechanical, thermal, and tribological properties. TP-8474 parts offer excellent strength and toughness, dimensional stability, low outgassing, radiation..
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
DIN 53752
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
DIN 53752
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
DIN 53752
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
Average value: 6.00 µm/m-°C Grade Count:6
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
DIN 53752
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
DIN 53752
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
DIN 53752
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Copyright © lookpolymers.com All Rights Reserved