Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific)
Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating..
CTE, linear, Transverse to Flow 77.0 - 160 µm/m-°C

@Temperature 55.0 - 250 °C
42.8 - 88.9 µin/in-°F

@Temperature 131 - 482 °F
Average value: 121 µm/m-°C Grade Count:8
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RX05049 PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RX05049 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Proprietary Lubricant. Added features include; Internally Lubricated.
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP
LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic..
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WX93111 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WX93111 is a compound based on Polybutylene Terephalate resin containing Flame retardant , Glass Fiber, Proprietary filler. Added features include : Improved CTI.
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East)
LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON KD000EI Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Kon* KD000EI is a compound based on Acetal Copolymer resin containing Carbon Powder. Added features include: Electrically Conductive, Impact Modified.
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature 55.0 - 160 °C
42.8 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 77.0 µm/m-°C
42.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly..
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON RX00327 PA 66
LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural.