Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 17.0 - 50.0 µm/m-°C
9.44 - 27.8 µin/in-°F
Average value: 36.3 µm/m-°C Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
CTE, linear, Transverse to Flow 24.0 - 50.0 µm/m-°C
13.3 - 27.8 µin/in-°F
Average value: 30.2 µm/m-°C Grade Count:33
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 2923 W Novolac Phenolic
Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X681 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica..
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 2530 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba..
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 2723 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre..
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 2920 W Novolac Phenolic
Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B..
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF