Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 17.0 - 80.0 µm/m-°C
9.44 - 44.4 µin/in-°F
Average value: 55.4 µm/m-°C Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear, Transverse to Flow 17.0 - 50.0 µm/m-°C
9.44 - 27.8 µin/in-°F
Average value: 36.3 µm/m-°C Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
CTE, linear, Transverse to Flow 17.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
9.44 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP610 Paper Base Laminate
Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne..
CTE, linear, Transverse to Flow 17.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
9.44 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP611 Paper Base Laminate
Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a..