Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.1 - 18.1 µm/m-°C @Temperature 20.0 - 200 °C |
9.50 - 10.1 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |