Thermal Properties Metric English Comments
CTE, linear 17.1 - 18.1 µm/m-°C

@Temperature 20.0 - 200 °C
9.50 - 10.1 µin/in-°F

@Temperature 68.0 - 392 °F
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..