CTE, linear 10.35 µm/m-°C

@Temperature 21.0 - 149 °C
5.750 µin/in-°F

@Temperature 69.8 - 300 °F
Crucible Steel 154 CM Martensitic Steel
Crucible 154 CM is a modification of 440C martensitic stainless steel to which molybdenum has been added. 154 CM has better corrosion resistance, better wear resistance and better hot-hardness than ..
CTE, linear 10.35 µm/m-°C

@Temperature 21.0 - 149 °C
5.750 µin/in-°F

@Temperature 69.8 - 300 °F
Crucible Steel CPM® 154 Tool Steel
CPM 154 is CPM-manufactured version of Crucible’s standard 154 CM. The CPM manufacturing process produces a uniform distribution of the carbides in this grade, giving this CPM 154 easier grinding a..