Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.91 µm/m-°C @Temperature 21.0 - 260 °C |
6.061 µin/in-°F @Temperature 69.8 - 500 °F |
|
Crucible Steel 154 CM Martensitic Steel Crucible 154 CM is a modification of 440C martensitic stainless steel to which molybdenum has been added. 154 CM has better corrosion resistance, better wear resistance and better hot-hardness than .. |
|||
CTE, linear | 10.91 µm/m-°C @Temperature 21.0 - 260 °C |
6.061 µin/in-°F @Temperature 69.8 - 500 °F |
|
Crucible Steel CPM® 154 Tool Steel CPM 154 is CPM-manufactured version of Crucible’s standard 154 CM. The CPM manufacturing process produces a uniform distribution of the carbides in this grade, giving this CPM 154 easier grinding a.. |