Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 23.0 - 60.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murytal® C Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
CTE, linear 110 µm/m-°C

@Temperature 23.0 - 100 °C
61.1 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive
Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•..
CTE, linear 110 µm/m-°C

@Temperature 23.0 - 100 °C
61.1 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
CTE, linear 110 - 120 µm/m-°C

@Temperature 25.0 - 200 °C
61.1 - 66.7 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
CTE, linear 110 µm/m-°C

@Temperature >=143 °C
61.1 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..
CTE, linear 110 µm/m-°C

@Temperature >=143 °C
61.1 µin/in-°F

@Temperature >=289 °F
ISO 11359
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
CTE, linear 110 µm/m-°C

@Temperature >=143 °C
61.1 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
CTE, linear 110 µm/m-°C

@Temperature >=143 °C
61.1 µin/in-°F

@Temperature >=289 °F
Average above Tg; ASTM D696
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
CTE, linear 110 µm/m-°C

@Temperature >=143 °C
61.1 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
CTE, linear 110 µm/m-°C

@Temperature >=152 °C
61.1 µin/in-°F

@Temperature >=306 °F
Average above Tg; ISO 11359
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
CTE, linear 110 µm/m-°C

@Temperature 200 - 300 °C
61.1 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
3M Dyneon™ 1750 PTFE Powder  (discontinued **)
Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r..
CTE, linear 110 µm/m-°C

@Temperature 200 - 300 °C
61.1 µin/in-°F

@Temperature 392 - 572 °F
ASTM D1530
3M Dyneon™ 1620 PTFE Powder  (discontinued **)
Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
CTE, linear 110 µm/m-°C

@Temperature 200 - 300 °C
61.1 µin/in-°F

@Temperature 392 - 572 °F
ASTM E1530
3M Dyneon™ 1641 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
CTE, linear 110 µm/m-°C

@Temperature 200 - 300 °C
61.1 µin/in-°F

@Temperature 392 - 572 °F
ASTM E1530
3M Dyneon™ 1645 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
CTE, linear 110 µm/m-°C

@Temperature -60.0 - 50.0 °C
61.1 µin/in-°F

@Temperature -76.0 - 122 °F
DIN 53122
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
CTE, linear 110 µm/m-°C

@Temperature >=103 °C
61.1 µin/in-°F

@Temperature >=217 °F
above Tg
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
CTE, linear 110 µm/m-°C

@Temperature >=34.0 °C
61.1 µin/in-°F

@Temperature >=93.2 °F
above Tg
Resinlab® SEC1222 Silver Filled Epoxy Adhesive
Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit..
CTE, linear 110 µm/m-°C

@Temperature 100 °C
61.1 µin/in-°F

@Temperature 212 °F
Estimated by MatWeb from similar grades
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro..
CTE, linear 110 µm/m-°C

@Temperature >=143 °C
61.1 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..
CTE, linear 110 µm/m-°C

@Temperature >=143 °C
61.1 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..