Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.2 µm/m-°C @Temperature -5.00 - 25.0 °C |
16.8 µin/in-°F @Temperature 23.0 - 77.0 °F |
ASTM E228 |
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b.. |