Polymer Property : CTE, linear = 30.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 30.2 µm/m-°C

@Temperature -5.00 - 25.0 °C
16.8 µin/in-°F

@Temperature 23.0 - 77.0 °F
ASTM E228
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound
An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b..