Thermal Properties Metric English Comments
CTE, linear 55.1 µm/m-°C

@Temperature 23.0 - 150 °C
30.6 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E831
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet)
KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. ..
CTE, linear 55.1 µm/m-°C

@Temperature 23.0 - 150 °C
30.6 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E831
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet)
KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re..
CTE, linear 55.0 µm/m-°C

@Temperature <=143 °C
30.6 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
CTE, linear 55.0 µm/m-°C

@Temperature <=143 °C
30.6 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
CTE, linear 55.0 µm/m-°C

@Temperature <=143 °C
30.6 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
CTE, linear 55.0 µm/m-°C

@Temperature <=143 °C
30.6 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
CTE, linear 55.0 µm/m-°C

@Temperature <=143 °C
30.6 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 90G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
CTE, linear 55.0 µm/m-°C

@Temperature <=152 °C
30.6 µin/in-°F

@Temperature <=306 °F
Average below Tg; ISO 11359
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
CTE, linear 55.0 µm/m-°C

@Temperature <=162 °C
30.6 µin/in-°F

@Temperature <=324 °F
Average below Tg; ISO 11359
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
CTE, linear 55.0 µm/m-°C

@Temperature 23.0 °C
30.6 µin/in-°F

@Temperature 73.4 °F
MD; ASTM D696
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear 55.0 µm/m-°C

@Temperature 200 °C
30.6 µin/in-°F

@Temperature 392 °F
MD; ASTM D696
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear 55.0 µm/m-°C

@Temperature 30.0 - 100 °C
30.6 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
3M Dyneon™ CC503 PTFE, 15% Mineral Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings - FDA compliant, valve seats, seals.Data provided by Dyneon.
CTE, linear 55.1 µm/m-°C

@Temperature 121 °C
30.6 µin/in-°F

@Temperature 250 °F
ASTM D696
Dow SPECTRIM™ HH 390 Reaction Moldable Polymer
Information provided by Dow
CTE, linear 55.0 µm/m-°C

@Temperature -80.0 - 70.0 °C
30.6 µin/in-°F

@Temperature -112 - 158 °F
ASTM D686-79
Arkema Group VOLTALEF® 300 HD PCTFE
VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group
CTE, linear 55.0 µm/m-°C

@Temperature -80.0 - 70.0 °C
30.6 µin/in-°F

@Temperature -112 - 158 °F
ASTM D686-79
Arkema Group VOLTALEF® 302 PCTFE
VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group
CTE, linear 55.0 µm/m-°C

@Temperature 23.0 - 100 °C
30.6 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murpec® Polyetheretherketone
In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change..
CTE, linear 55.1 µm/m-°C

@Temperature 50.0 - 185 °C
30.6 µin/in-°F

@Temperature 122 - 365 °F
Z-Axis Alpha 1; IPC-TM-650.2.4.41
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy
The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW..
CTE, linear 55.0 µm/m-°C

@Temperature <=143 °C
30.6 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
CTE, linear 55.0 µm/m-°C

@Temperature <=143 °C
30.6 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..
Copyright © lookpolymers.com All Rights Reserved