Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 70.2 µm/m-°C @Temperature 20.0 °C |
39.0 µin/in-°F @Temperature 68.0 °F |
Across Thickness; ASTM D-696 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |