Thermal Properties Metric English Comments
CTE, linear 70.2 µm/m-°C

@Temperature 20.0 °C
39.0 µin/in-°F

@Temperature 68.0 °F
Across Thickness; ASTM D-696
Glastic GLASTHERM S Insulation Sheet
Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e..