Polymer Property : CTE, linear = 40.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 73.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
40.6 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
3D Systems Accura® 50 Plastic for SLA® Systems
Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te..
CTE, linear 73.0 µm/m-°C

@Temperature -50.0 - 0.000 °C
40.6 µin/in-°F

@Temperature -58.0 - 32.0 °F
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M