Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 73.0 µm/m-°C @Temperature 0.000 - 20.0 °C |
40.6 µin/in-°F @Temperature 32.0 - 68.0 °F |
T<Tg; ASTM E831-93 |
3D Systems Accura® 50 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te.. |
|||
CTE, linear | 73.0 µm/m-°C @Temperature -50.0 - 0.000 °C |
40.6 µin/in-°F @Temperature -58.0 - 32.0 °F |
|
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |