Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.0 µm/m-°C @Temperature 100 °C |
5.56 µin/in-°F @Temperature 212 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
CTE, linear | 10.0 - 14.0 µm/m-°C @Temperature -40.0 - 125 °C |
5.56 - 7.78 µin/in-°F @Temperature -40.0 - 257 °F |
X/Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 20.0 - 900 °C |
5.56 µin/in-°F @Temperature 68.0 - 1650 °F |
|
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 900 °C |
5.56 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ) Brand 868 features: High density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal c.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 20.0 - 100 °C |
5.56 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 20.0 - 300 °C |
5.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-FK5 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XE4050BL Polyphenylene Sulfide Alloy Xtel® XE4050BL is a glass fiber and mineral filled PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevron Phillips.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 21.0 - 500 °C |
5.56 µin/in-°F @Temperature 69.8 - 932 °F |
Mean |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 200 °C |
5.56 µin/in-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 100 °C |
5.56 µin/in-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 100 °C |
5.56 µin/in-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 50.0 - 150 °C |
5.56 µin/in-°F @Temperature 122 - 302 °F |
x direction; IPC TM-650 2.4.41 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 0.000 - 100 °C |
5.56 µin/in-°F @Temperature 32.0 - 212 °F |
x direction; IPC TM-650 2.4.24 |
Arlon CLTE-P Pre-Preg Bonding Layer Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of .. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 20.0 - 100 °C |
5.56 µin/in-°F @Temperature 68.0 - 212 °F |
|
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2) Speed Star high speed steel in a fine-grained "Moly"-Tungsten high-speed steel manufactured under close control. It has certain advantages over 18-4-1 high speed steels, some of which are lower cost.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature -100 °C |
5.56 µin/in-°F @Temperature -148 °F |
|
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 20.0 - 300 °C |
5.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG28 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.0 µm/m-°C @Temperature 20.0 - 200 °C |
5.56 µin/in-°F @Temperature 68.0 - 392 °F |
|
Latrobe LSS™ 440C Stainless Steel Knife (ASTM A276) TLS 440C Stainless Knife Steel is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 60 HRC. The high carbon content results in a hard matrix and numero.. |