CTE, linear 93.0 µm/m-°C

@Temperature 200 - 300 °C
51.7 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
3M Dyneon™ TFM™ 1705 Modified PTFE Powder  (discontinued **)
Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat..
CTE, linear 93.0 µm/m-°C

@Temperature 25.0 - 80.0 °C
51.7 µin/in-°F

@Temperature 77.0 - 176 °F
DIN 53752
Styron INSPIREâ„¢ TF0808S(U) Polypropylene
TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE ..
CTE, linear 93.0 µm/m-°C

@Temperature 0.000 - 50.0 °C
51.7 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
DSM Somos® 14120 Water-resistant resin for stereolithography, White
DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p..
CTE, linear 93.0 µm/m-°C

@Temperature 5.00 - 20.0 °C
51.7 µin/in-°F

@Temperature 41.0 - 68.0 °F
Below Tg
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb..
CTE, linear 93.0 µm/m-°C

@Temperature 20.0 - 100 °C
51.7 µin/in-°F

@Temperature 68.0 - 212 °F
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate
A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL)