Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 93.0 µm/m-°C @Temperature 200 - 300 °C |
51.7 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ TFM™ 1705 Modified PTFE Powder
(discontinued **) Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat.. |
|||
CTE, linear | 93.0 µm/m-°C @Temperature 25.0 - 80.0 °C |
51.7 µin/in-°F @Temperature 77.0 - 176 °F |
DIN 53752 |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
CTE, linear | 93.0 µm/m-°C @Temperature 0.000 - 50.0 °C |
51.7 µin/in-°F @Temperature 32.0 - 122 °F |
ASTM E831-00 |
DSM Somos® 14120 Water-resistant resin for stereolithography, White DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p.. |
|||
CTE, linear | 93.0 µm/m-°C @Temperature 5.00 - 20.0 °C |
51.7 µin/in-°F @Temperature 41.0 - 68.0 °F |
Below Tg |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
CTE, linear | 93.0 µm/m-°C @Temperature 20.0 - 100 °C |
51.7 µin/in-°F @Temperature 68.0 - 212 °F |
|
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL) |