Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 199 °C |
6.10 µin/in-°F @Temperature 68.0 - 390 °F |
|
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 316 °C |
6.10 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.10 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel CHRO-MOW® Tool Steel, AISI H12 Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants ar.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.10 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel CPM® Nu-Die® EZ Tool Steel CRUCIBLE CPM Nu-Die EZ is a new, patented die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition, and is easily machined.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 204 °C |
6.10 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19 Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 204 °C |
6.10 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel PEERLESS A Tool Steel, AISI H21 Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 199 °C |
6.10 µin/in-°F @Temperature 390 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 199 °C |
6.10 µin/in-°F @Temperature 390 °F |
hardened to 50 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 600.0 °C |
6.10 µin/in-°F @Temperature 1112 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.10 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr.. |