Material Notes:
Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Uddeholm Stavax ESR is recommended for all types of moulding tools and its special proper­ ties make it particularly suitable for moulds with the following demands:Corrosion/staining resistance, i.e. for moulding of corrosive materials, e.g. PVC, acetates, and for moulds subjected to humid working/storage conditions.Wear resistance, i.e. for moulding abrasive/ filled materials, including injection-moulded thermosetting grades. Uddeholm Stavax ESR is recommended for moulds with long production runs, e.g. disposable cutlery and containers.High surface finish, i.e. for the production of optical parts, such as camera and sun­ glasses lenses, and for medical containers, e.g. syringes, analysis phials.
Physical Properties Metric English Comments
Density 7.81 g/cc
0.282 lb/in³
hardened to 50 HRC
7.67 g/cc

@Temperature 399 °C
0.277 lb/in³

@Temperature 750 °F
hardened to 50 HRC
7.75 g/cc

@Temperature 199 °C
0.280 lb/in³

@Temperature 390 °F
hardened to 50 HRC
Mechanical Properties Metric English Comments
Hardness, Brinell 200
200
Soft annealed (Delivery condition)
Hardness, Rockwell C 30 - 55
30 - 55
tempering temp 200 - 1200°F
Tensile Strength, Ultimate 1420 MPa
206000 psi
hardened to 45 HRC
1770 MPa
256000 psi
hardened to 50 HRC
Tensile Strength, Yield 1280 MPa

@Strain 0.200 %
185000 psi

@Strain 0.200 %
hardened to 45 HRC
1470 MPa

@Strain 0.200 %
213000 psi

@Strain 0.200 %
hardened to 50 HRC
Modulus of Elasticity 200 GPa
29000 ksi
(hardened to 50 HRC)
180 GPa

@Temperature 399 °C
26100 ksi

@Temperature 750 °F
hardened to 50 HRC
190 GPa

@Temperature 199 °C
27600 ksi

@Temperature 390 °F
hardened to 50 HRC
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 199 °C
6.10 µin/in-°F

@Temperature 390 °F
hardened to 50 HRC
11.3 µm/m-°C

@Temperature 399 °C
6.30 µin/in-°F

@Temperature 750 °F
hardened to 50 HRC
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
hardened to 50 HRC
Thermal Conductivity 16.0 W/m-K

@Temperature 20.0 °C
111 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
hardened to 50 HRC
20.0 W/m-K

@Temperature 199 °C
139 BTU-in/hr-ft²-°F

@Temperature 390 °F
hardened to 50 HRC
24.0 W/m-K

@Temperature 399 °C
167 BTU-in/hr-ft²-°F

@Temperature 750 °F
hardened to 50 HRC
Component Elements Properties Metric English Comments
Carbon, C 0.38 %
0.38 %
Chromium, Cr 13.6 %
13.6 %
Iron, Fe 84.3 %
84.3 %
as balance
Manganese, Mn 0.50 %
0.50 %
Silicon, Si 0.90 %
0.90 %
Vanadium, V 0.30 %
0.30 %