Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 300 °C |
7.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
International Mold Steel NAK80 Precipitation Hardened Mold Steel Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, u.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 200 °C |
7.50 µin/in-°F @Temperature 68.0 - 392 °F |
|
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24 Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® W alloy, gas tungsten arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® W alloy, shielded metal arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 538 °C |
7.50 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 100 °C |
7.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 200 °C |
7.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® alloy 718 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® alloy X 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 649 °C |
7.50 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 200 °C |
7.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
HP Alloys Alloy 718, 0% Cold Worked, Not Aged 0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes .. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 200 °C |
7.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
HP Alloys Alloy 718, 30% Cold Worked, Aged 30% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 200 °C |
7.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
HP Alloys Alloy 718, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.1 - 204 °C |
7.50 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700.0 °C |
7.50 µin/in-°F @Temperature 68.0 - 1292 °F |
|
Schmolz + Bickenbach Thermodur® 2999 Hot Work Die Steel Description: Maximum high-temperature strength, good high-temperature wear resistance, excellent thermal shock resistance and thermal conductivity across the entire range of service temperatures App.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 500 °C |
7.50 µin/in-°F @Temperature 69.8 - 932 °F |
Mean |
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 0.000 - 649 °C |
7.50 µin/in-°F @Temperature 32.0 - 1200 °F |
|
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008) Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 0.000 - 100 °C |
7.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® alloy 625 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 200 °C |
7.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
HP Alloys Alloy 718, 50% Cold Worked, Aged 50% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 427 °C |
7.50 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |