Haynes Hastelloy® alloy 718 12.7 mm plate weldments

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Haynes International, Inc.
Trade Name Hastelloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haynes Hastelloy® alloy 718 12.7 mm plate weldments.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemical process industries.Data provided by the manufacturer, Haynes International, Inc.
Physical Properties Metric English Comments
Density 9.00 g/cc
0.325 lb/in³
at RT
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 860 MPa
125000 psi
Tensile Strength, Yield 470 MPa
68200 psi
Elongation at Break 23 %
23 %
Failures in weld.
Reduction of Area 31 %
31 %
Failures in weld.
Thermal Properties Metric English Comments
CTE, linear 13.2 µm/m-°C

@Temperature 20.0 - 600 °C
7.33 µin/in-°F

@Temperature 68.0 - 1110 °F
13.2 µm/m-°C

@Temperature 20.0 - 500 °C
7.33 µin/in-°F

@Temperature 68.0 - 932 °F
13.5 µm/m-°C

@Temperature 20.0 - 700 °C
7.50 µin/in-°F

@Temperature 68.0 - 1290 °F
14.2 µm/m-°C

@Temperature 20.0 - 800 °C
7.89 µin/in-°F

@Temperature 68.0 - 1470 °F
14.8 µm/m-°C

@Temperature 20.0 - 900 °C
8.22 µin/in-°F

@Temperature 68.0 - 1650 °F
15.3 µm/m-°C

@Temperature 20.0 - 1000 °C
8.50 µin/in-°F

@Temperature 68.0 - 1830 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Chromium, Cr 5.0 %
5.0 %
Cobalt, Co 2.5 %
2.5 %
Iron, Fe 6.0 %
6.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 24 %
24 %
Nickel, Ni 63 %
63 %
Silicon, Si <= 1.0 %
<= 1.0 %
Vanadium, V <= 0.60 %
<= 0.60 %