Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 0.000 - 500 °C |
8.33 µin/in-°F @Temperature 32.0 - 932 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 0.000 - 500 °C |
8.33 µin/in-°F @Temperature 32.0 - 932 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 0.000 - 500 °C |
8.33 µin/in-°F @Temperature 32.0 - 932 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 0.000 - 500 °C |
8.33 µin/in-°F @Temperature 32.0 - 932 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 0.000 - 500 °C |
8.33 µin/in-°F @Temperature 32.0 - 932 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 4.8 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 0.000 - 500 °C |
8.33 µin/in-°F @Temperature 32.0 - 932 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 200 °C |
8.33 µin/in-°F @Temperature 68.0 - 392 °F |
|
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 500 °C |
8.33 µin/in-°F @Temperature 68.0 - 932 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 25.0 - 1000 °C |
8.33 µin/in-°F @Temperature 77.0 - 1830 °F |
|
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 25.0 - 1000 °C |
8.33 µin/in-°F @Temperature 77.0 - 1830 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 600 °C |
8.33 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 100 °C |
8.33 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 200 °C |
8.33 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 288°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 200 °C |
8.33 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 200 °C |
8.33 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 316°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 250 °C |
8.33 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |