Polymer Property : Maximum Service Temperature, Air = 164 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 164 °C

@Time 7.20e+7 sec
327 °F

@Time 20000 hour
Continuous; ASTM D3045
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Maximum Service Temperature, Air 164 °C

@Time 7.20e+7 sec
327 °F

@Time 20000 hour
Continuous; ASTM D3045
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..