Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 164 °C @Time 7.20e+7 sec |
327 °F @Time 20000 hour |
Continuous; ASTM D3045 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Maximum Service Temperature, Air | 164 °C @Time 7.20e+7 sec |
327 °F @Time 20000 hour |
Continuous; ASTM D3045 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |