Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 115 - 125 °C | 239 - 257 °F | ASTM D1525, HDT Method B |
Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 120 - 125 °C | 248 - 257 °F | ASTM D1525, HDT Method B |
Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.0 - 125 °C | 190 - 257 °F | Average value: 114 °C Grade Count:14 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |