Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler , Polypropylene, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.10 - 1.20 g/cc
1.10 - 1.20 g/cc
ASTM D792
Filler Content 40 %
40 %
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.0 - 28.0 MPa
3770 - 4060 psi
ASTM D683
Flexural Modulus 2.80 - 3.20 GPa
406 - 464 ksi
ASTM D790
Izod Impact, Notched 0.300 - 0.400 J/cm
0.562 - 0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 - 125 °C
248 - 257 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB