Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 49.0 - 53.0 °C | 120 - 127 °F | ASTM D648 |
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 49.0 - 53.0 °C | 120 - 127 °F | ASTM D648 |
3D Systems Accura® 50 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te.. |