Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 135 °C
194 - 275 °F
Average value: 113 °C Grade Count:14
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
Deflection Temperature at 0.46 MPa (66 psi) 125 - 135 °C
257 - 275 °F
ASTM D1525, HDT Method B
Loxim 830 12 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 125 - 135 °C
257 - 275 °F
ASTM D1525, HDT Method B
Loxim 830 01 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 51.1 - 135 °C
124 - 275 °F
Average value: 91.2 °C Grade Count:32
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..