Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 135 °C | 194 - 275 °F | Average value: 113 °C Grade Count:14 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 125 - 135 °C | 257 - 275 °F | ASTM D1525, HDT Method B |
Loxim 830 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 125 - 135 °C | 257 - 275 °F | ASTM D1525, HDT Method B |
Loxim 830 01 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 51.1 - 135 °C | 124 - 275 °F | Average value: 91.2 °C Grade Count:32 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |