Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 150 - 155 °C | 302 - 311 °F | ASTM D1525, HDT Method B |
Loxim 140 01V0 Polycarbonate, 40% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 145 - 155 °C | 293 - 311 °F | ASTM D1525, HDT Method B |
Loxim 830 01 HBCC Polypropylene Compound 30% Chemically Coupled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.9 - 155 °C | 210 - 311 °F | Average value: 148 °C Grade Count:26 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |