Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 176 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 - 80.0 °C
165 - 176 °F
with 160°C Thermal Postcure; ASTM D648
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer
Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey..
Deflection Temperature at 0.46 MPa (66 psi) 75.0 - 80.0 °C
167 - 176 °F
after thermal post treatment procedure A; ASTM D648-06
Proto3000 Objet RGD525 High Temperature Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
Deflection Temperature at 0.46 MPa (66 psi) 74.0 - 80.0 °C
165 - 176 °F
with 160ºC thermal postcure; ASTM D648
3D Systems Accura® 50 Plastic for SLA® Systems
Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te..
Deflection Temperature at 0.46 MPa (66 psi) 75.0 - 80.0 °C
167 - 176 °F
C.O.I.M. EXTER S® S 111 B Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 111 B: Low viscosity..
Deflection Temperature at 0.46 MPa (66 psi) 34.0 - 80.0 °C
93.2 - 176 °F
Average value: 45.3 °C Grade Count:24
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..