Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 224 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 204 - 224 °C
400 - 435 °F
Average value: 212 °C Grade Count:15
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Deflection Temperature at 0.46 MPa (66 psi) 207 - 224 °C
405 - 435 °F
Average value: 220 °C Grade Count:32
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Deflection Temperature at 0.46 MPa (66 psi) 210 - 224 °C
410 - 435 °F
Average value: 217 °C Grade Count:10
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Deflection Temperature at 0.46 MPa (66 psi) 182 - 224 °C
360 - 435 °F
Average value: 211 °C Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Deflection Temperature at 0.46 MPa (66 psi) 182 - 224 °C
360 - 435 °F
Average value: 202 °C Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..