Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 226 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 108 °C
158 - 226 °F
Average value: 87.8 °C Grade Count:31
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 108 °C
176 - 226 °F
Average value: 92.6 °C Grade Count:14
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..