Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 4008 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 4009 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 4015 THW Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **) ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Polymer Resources PC/TP-GP2-G20 PC Polyester, Excellent Chemical Resistance, 20% Glass Filled
(Unverified Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Ineos H20Z-00 Polypropylene Homopolymer This is a nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Appl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ISO 75 |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ASA GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ASA GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Spartech EP5240 Calcium Carbonate Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications inc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0096 S LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0096 S3 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0320 S1 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | unannealed; ASTM D648 |
Dow INSPIRE™ 117.00 Performance Polymer 117.00 Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Asahi Kasei Thermofil P6-9900-0570 Unfilled, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Aaron Industries AAROPRENE® TFPP 2010 Talc Filled Polypropylene AAROPRENE® TFPP 2000 Series Talc Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | Unannealed; ASTM D648 |
Multibase Multi-Flam™ 0106 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |