Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 30.3 MPa
4400 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.2 µm/m-°C
19.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
240 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257