Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 276 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 276 °C
529 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers
Deflection Temperature at 0.46 MPa (66 psi) 276 °C
529 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46
LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 276 °C

@Thickness 3.20 mm
529 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear
LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) 276 °C

@Thickness 3.20 mm
529 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp OFM66 PPS
LNP* Thermocomp* OFM66 is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP fo..
Deflection Temperature at 0.46 MPa (66 psi) 276 °C
529 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL BK083 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Deflection Temperature at 0.46 MPa (66 psi) 276 °C
529 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Deflection Temperature at 0.46 MPa (66 psi) 276 °C
529 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance..