Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 378 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
Unannealed; ASTM D648
PolyOne Gravi-Tech™ GRV-NY-085-W-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
Covestro Apec® DP 1-9379/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
ISO 75-1,-2
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66
PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 6.40 mm
378 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 6.40 mm
378 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA11 GF30 TL20 LE 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Good Wear Resistance, Low Extractables, Lubricat..
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific)
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
ASTM D648
Samyang Tramid® 910 PA66/PA6
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.Applications:Automotive knob types, door handles and mirror housingsConnectorsCab..
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP V1000UXC PA
LNP* Thermotuf* V1000UXC is a compound based on Nylon resin. Added features of this material include: UV Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 6
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 6.40 mm
378 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
ISO 75-1/-2
Covestro Apec® 2095 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
dry; ISO 75-1/-2
DSM Novamid® 1010N2 1ES NAT PA6 FR(30)
Injection Molding, Flame Retardant (Halogen free)
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
ASTM D648
A. Schulman ComAlloy Lubrilon® 605 Nylon 6/6, PTFE Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
ASTM D648
A. Schulman ComAlloy Voloy® 612 Nylon 6, Glass Fiber/Bead Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermotuf V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific)
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6
LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity.
Deflection Temperature at 0.46 MPa (66 psi) 192 °C

@Thickness 3.20 mm
378 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.