Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 225 °C
194 - 437 °F
Average value: 138 °C Grade Count:44
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Deflection Temperature at 0.46 MPa (66 psi) 138 - 225 °C
280 - 437 °F
Average value: 214 °C Grade Count:101
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Deflection Temperature at 0.46 MPa (66 psi) 169 - 225 °C
336 - 437 °F
Average value: 212 °C Grade Count:87
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Deflection Temperature at 0.46 MPa (66 psi) 215 - 225 °C
419 - 437 °F
ASTM D1525, HDT Method B
Loxim 235 01V0 Polybutylene Terephthalate
Information provided by Loxim Industries