Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Lubricomp JX91055 PES (Europe-Africa-Middle East) LNP* LUBRICOMP* JX91055 is a compound based on Polyethersulfone resin containing Carbon Fiber and Proprietary Lubricant . Added features include Internally Lubricated and Electrically Conductive.Thi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific) LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
Cheng Yu Plastic T889G25 PBT, 25% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
Adell AJ-13 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
Ashley Polymers Ashlene® 526LD Nylon 66 Modified for toughness at low temperatures, injection molding grade.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 415 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 631 Nylon 6/6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |