Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 244 °C | 471 °F | ASTM D648 |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 244 °C | 471 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 244 °C @Thickness 3.20 mm |
471 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 244 °C | 471 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 244 °C | 471 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |