Aclo Accuguard Polypropylene HPN469V2CSL Homopolymer Non-Halogenated Copper Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Aclo Compounders
Trade Name Accuguard
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accuguard Polypropylene HPN469V2CSL Homopolymer Non-Halogenated Copper Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
MD; ASTM D955
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 35 %
35 %
ASTM D638
Tensile Modulus 1.900 GPa
275.5 ksi
ASTM D638
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Flexural Modulus 1.900 GPa
275.5 ksi
ASTM D790
Izod Impact, Notched 0.272 J/cm
0.510 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C
196 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.1 °C
133 °F
Flammability, UL94 V-2

@Thickness 1.59 mm
V-2

@Thickness 0.0625 in
UL File #E99379
Users viewing this material also viewed the following: