Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 50.0 - 120 °C | 122 - 248 °F | Average value: 91.0 °C Grade Count:14 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
UL RTI, Mechanical with Impact | 65.0 - 120 °C | 149 - 248 °F | Average value: 90.7 °C Grade Count:11 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
UL RTI, Mechanical with Impact | 65.0 - 120 °C | 149 - 248 °F | Average value: 76.0 °C Grade Count:9 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |