Thermal Properties Metric English Comments
Pour Point -97.0 °C
-143 °F
Solvay Specialty Polymers Galden® D02 PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Pour Point -97.0 °C
-143 °F
Solvay Specialty Polymers Galden® D02TS PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Pour Point <= -97.0 °C
<= -143 °F
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Pour Point -97.0 °C
-143 °F
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..