Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -97.0 °C | -143 °F | |
Solvay Specialty Polymers Galden® D02 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Pour Point | -97.0 °C | -143 °F | |
Solvay Specialty Polymers Galden® D02TS PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Pour Point | <= -97.0 °C | <= -143 °F | |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Pour Point | -97.0 °C | -143 °F | |
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |