Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 5.99 mm |
149 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**) Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.800 mm |
149 °F @Thickness 0.0315 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 253 Nylon 6, Toughened Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL746B |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG6 PA66, 30% Glass Filled, Injection Molded AG6 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.810 mm |
149 °F @Thickness 0.0319 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |