Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.59 mm |
149 °F @Thickness 0.0625 in |
UL 746 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.17 mm |
149 °F @Thickness 0.125 in |
UL 746 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=0.820 mm |
149 °F @Thickness >=0.0323 in |
|
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL746B |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
UL 746 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
UL 746B |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |