Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 5.99 mm |
149 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**) Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 6.00 mm |
149 °F @Thickness 0.236 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66
(Unverified Data**) Zytel® 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.800 mm |
149 °F @Thickness 0.0315 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=3.00 mm |
149 °F @Thickness >=0.118 in |
|
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-G6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
|
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |