Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -14.0 °C | 6.80 °F | Wide variability between samples is observed.; ASTM D746 |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D746-79 |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D746 |
Chevron Phillips Marlex® 1409 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D746 |
Teknor Apex APEX® 80102 Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS Compliant Uses: InsulationAgency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire Types: TWInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | |
Daikin DAI-EL G-603 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Information provided by Daikin Industries. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D746 |
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D746 |
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D-746 |
Axiall 19871 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistance applications.Information provided by Georgia GulfGeorgia Gulf bec.. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D-746 |
Axiall 2161A Wire & Cable Flexible PVC Flame retardant, oil resistant, 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098A-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | |
Sylvin Technologies 6055 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -14.0 °C | 6.80 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W649LF Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |